~/talk

Melting metal for fun and profit

Talkat DEF CON 23 · 2015-08-06..08-09· [embedded-and-hardware]
links:none on file
slides:none on file

Covers practical soldering: 60/40 tin/lead mix is near the eutectic at about 168°C and is easier than lead‑free tin/silver/copper; rosin flux is the weak organic acid that removes copper oxide and prevents nonwetting; aim for concave shiny joints, heat both pad and wire, feed solder from the far side and leave the iron a second after removing solder; use rosin flux (no‑clean) and clean with 91% IPA if sticky; recommended tool is hot air + soldering station ($100–200) with temperature control.

AI-written summary · about

  1. 0:00Introduction to soldering
  2. 0:42What is solder made of
  3. 2:06Lead vs lead-free solder
  4. 2:27How flux makes soldering work
  5. 3:53Flux and copper oxide reaction
  6. 4:56Surface tension in soldering
  7. 5:39Choosing a soldering iron
  8. 6:43What a good solder joint looks like
  9. 8:30Proper soldering technique
  10. 10:38How solder is constructed
  11. 11:19Cleaning flux residue
  12. 11:40Soldering contest and resources
~/search
type to search 8,222 conferences, 162,397 speakers and 219,688 talks
~/help
cmdctrl k
search every conference, speaker and series
/
focus the filter search
h
home
c
conferences
s
speakers
e
series
t
light / dark — the status bar button does the same
← →
on a talk: 5 seconds back / forward
0–9
on a talk: jump to 0%–90% of the recording
?
this help
esc
close this, then clear every filter — or just the search, while you are typing in it

Ignored while you are typing. Pages without a filter rail have no search to focus.