Shows how to reliably reflow through‑hole (THT/THR) parts on mixed SMD/THT boards by using liquid crystal polymer (LCP) housings, shortening pins and adding a 0.3–0.5 mm standoff, and by increasing THT stencil apertures (up to ~30% more paste) and tuning convection profile so boards pass in one reflow. Presents data and examples achieving clean menisci and >75% through‑fill, references the industrial Class 3 spec (330°C / ≥74% fill), and provides the Excel calculator used to size paste volumes.